Home / All / Steel Forgings /

AISI O2 DIN 1.2842 Cold Work Tool Steel Round Bar

AISI O2 DIN 1.2842 Cold Work Tool Steel Round Bar

AISI O2 DIN 1.2842 Cold Work Tool Steel Round Bar
AISI O2 DIN 1.2842 Cold Work Tool Steel Round BarAISI O2 DIN 1.2842 Cold Work Tool Steel Round BarAISI O2 DIN 1.2842 Cold Work Tool Steel Round BarAISI O2 DIN 1.2842 Cold Work Tool Steel Round Bar
CategoriesSteel Forgings
Brandfushun
ModelO2 1.2842
Round bar8mm-350mm
Flat barthickness 2mm –300mm x width 200mm – 800mm
Surface FinishBlack, Rough Machined, Turned or as per given requirements.
Unit PriceUS $ 1500 / metric ton
FOB portSHANGHAI
Terms of PaymentL/C, T/T
Update TimeMar 28,2024
Detail Information

Applications for ASTM A681 O2 Tool Steel

Steel O2 is used as tool steel for universal use, highly stressed plastic moulds, mould inserts for high hardness and abrasive stress, blanking and stamping tools for all types cutting sheet metals up to 6 mm thickness, cold forming dies, cutting and punching tools of all types, shear blades for paper, plastic and metalworking industries, reamers, thread chasers and cutting tools, pressure pads, guide pins, taps, measuring tools, precision calipers and plug gauges, woodworking tools, plastic and rubber compression moulds, deep drawing tools, clipping.

Contact us for any request of O2 tool steel materials. We will be a better choice.

Standard

1. Relevant Steel Specification of AISI O2 Tool Steel

USA

German

British

China

ASTM A681

DIN EN ISO 4957

BS 4659

GB/T 1299

O2 / T31502

1.2842 / 90MnCrV8

B02

9Mn2V

2. AISI O2 Tool Steel Chemical Composition & Other Equivalents

ASTM A681

C

Mn

P

S

Si

Cr

V

Mo

O2 / T31502

0.85

0.95

1.40

1.80

0.03

0.03

. . .

0.50

. . .

0.50

. . .

0.30

. . .

0.30

DIN ISO 4957

C

Mn

P

S

Si

Cr

V

Mo

1.2842 / 90MnCrV8

0.85

0.95

1.80

2.20

0.03

0.03

0.10

0.40

0.20

0.50

0.05

0.20

. . .

. . .

BS 4659

C

Mn

P

S

Si

Cr

V

Mo

B02

0.85

0.95

1.50

1.80

0.035

0.035

. . .

0.40

. . .

. . .

. . .

0.25

. . .

. . .

GB/T 1299

C

Mn

P

S

Si

Cr

V

Mo

9Mn2V

0.85

0.95

1.70

2.00

0.03

0.03

. . .

0.40

. . .

. . .

0.10

0.25

. . .

. . .

3. ASTM O2 Tool Steel Material Mechanical Properties

 Forging of ASTM O2 Tool Steel

Heat O2 steel to 1000°C. Forge it within a range of 850-1050°C reheating if necessary. Cool slowly to avoid setting up stresses

5. AISI O2 Tool Steel Heat Treatment

Annealing : 680 – 720 °C

Hardness after annealing : Max. 220 HB

Stress relieving : Approx. 650 °C

Hot forming : 1050 – 850 °C

Hardening : 790 – 820 °C

Quenching media : Oil, Salt bath ( 220 – 250 °C ) up to 20 mm thickness

Hardness after quenching : 63 – 65 HRC

Hardness after tempering :

100℃

200℃

300℃

400℃

64HRC

62HRC

57HRC

50HRC

Please send your message to us
*Email
Tel
*Title
*Content
Upload
  • Only supports .rar/.zip/.jpg/.png/.gif/.doc/.xls/.pdf, maximum 20MB.
CONTACT PERSON
Name:
Florence Tang
Tel:

86-731-89903933

Email:
Address:
ADD: No. 812-813, Floor 8, Building C2, Yongsheng Commercial Plaza, 222 Labor East Road, Yuhua District, Changsha City, Hunan, China.
NEWSLETTER

sign up for the latest catalogue, new design and promotion

follow us